Coating exterior joinery before the Irish autumn

Exterior joinery fails at the joints and the end grain long before the face of the timber. Here is how to build a Sikkens system that lasts an Irish winter, and why late summer is the time to get it right.

A front door or a sash window spends its life in Irish rain, wind and low winter sun. The face of the timber usually copes. Failure starts at the joints, the end grain and the bottom rail, where water sits and soaks in. A good exterior system is built to stop that, and it is easier to build properly in late summer than in November.

Why exterior joinery fails

When exterior coatings fail early, the cause is usually one of these:

  • Unsealed end grain. End grain draws water in along the fibres. The timber swells and shrinks, and the coating cracks at the joint.
  • Wet timber. Coating timber that has not dried out traps moisture under the film. It finds its way out by lifting the coating.
  • A mixed system. An interior primer under an exterior topcoat, or products from different ranges, may not bond or move together.
  • Too little film. One coat of topcoat on bare timber is a decoration, not a protection.

None of these is fixed by a better topcoat. They are fixed by the steps that come before it.

Build the system in order

A typical Sikkens joinery system for windows and doors runs in this order. The exact products depend on the timber and whether you want a transparent or opaque finish, so confirm the system with the technical data sheets before you start.

  1. Impregnate. Cetol WP567 is a biocidal impregnation stain. It soaks into the timber to protect it rather than forming a film on top.
  2. Fill. Fill defects and nail holes with Kodrin WV442 joinery filler.
  3. Seal the end grain. Kodrin WV456 is an end-grain sealer. Apply it to cut ends, joints and the bottom of door and sash rails before assembly where you can.
  4. Prime or seal. For opaque finishes, use a primer such as the single-pack Rubbol WP 198 or the two-pack XP650 Aqua PU Primer, which takes 933 hardener at 1 litre to 5 litres. For transparent finishes, Cetol WF960 is a waterborne sealer in clear and light oak.
  5. Topcoat. Rubbol WF 3311 is a 25% sheen exterior topcoat in clear and white Promatch bases, tinted to the colour you need.

Stay in one system from impregnation to topcoat. The products are designed to bond to each other and to move with the timber together.

Get the timber right first

Before the first coat:

  • Check the moisture content. Use a moisture meter on the timber you are about to coat, not just one board from the stack. The system data sheet gives the maximum moisture content.
  • Sand to the grade the system asks for and remove the dust. Exterior coatings do not hide poor preparation.
  • Round sharp edges slightly. Coatings pull thin over a sharp arris and fail there first.

Why timing matters

Most exterior Sikkens joinery products are waterborne. Waterborne films need warmth and reasonably dry air to form properly. In cold, damp weather they dry slowly, and below the minimum temperature on the data sheet they may not form a sound film at all.

That is why late summer and early autumn is the time to get exterior work coated, whether it is going out on site or into a workshop-finished order. Factory-finished joinery coated in a warm, dry workshop and allowed to dry fully before delivery will outlast the same system rushed out in December.

If you do need to coat later in the year, coat indoors, keep the workshop and the timber above the minimum temperature on the data sheet, and give each coat its full drying time before the next. Our guide to spraying in a cold workshop covers heating for the drying time, not just the spraying.

Plan for maintenance

No exterior coating lasts forever. The aim is to maintain it before it fails, while a clean and recoat is still enough. Tell your customers to check south- and west-facing joinery once a year, especially bottom rails and sills, and to touch in any damage before water gets behind the film.

Colour and supply

We tint Rubbol WF 3311 Promatch in Tullamore and keep the formula on file, so the second batch for the same house matches the first. Bring a sample or a colour reference, or build a quote for the full system so the impregnation stain, sealer, primer and topcoat arrive together. More on keeping colours consistent is in colour matching that still matches on the second batch.

Questions from the counter

What is the right order for a Sikkens exterior joinery system?

A typical system is impregnation stain, filling, end-grain sealing, a primer or sealer, then the topcoat. For example: Cetol WP567, Kodrin WV442 filler, Kodrin WV456 edge sealer, a Rubbol or XP650 primer, then Rubbol WF 3311. Confirm the exact system for the timber and finish with the technical data sheets.

Why does exterior paint fail at the joints first?

End grain and joints absorb water far faster than the face of the timber. If the end grain is not sealed, moisture gets in behind the coating, the timber moves, and the film cracks and lifts at the joint.

Can I coat exterior joinery in cold or damp weather?

Waterborne exterior systems need dry timber and enough warmth to form a proper film. Cold, damp conditions slow drying and can stop the film forming properly. Check the minimum temperature on the data sheet and avoid coating when the timber is wet or dew is likely.

Does Lacquerite colour match Sikkens Rubbol topcoats?

Yes. Rubbol WF 3311 Promatch comes in clear and white bases at 25% sheen and can be tinted in Tullamore to the colour you need.

Apply this on a job

Tell sales the system, sheen, colour and when you need it on the gun.

Get a trade quote

Open a trade account today.